30-600MM/S PRINTING SPEED: With enhanced fluidity, ELEGOO RAPID PLA+ filament melts rapidly and flows smoothly, allowing for up to 600mm/s fast printing speed. You can complete the projects quickly without compromising on quality
ENHANCED STRENGTH & TOUGHNESS: ELEGOO RAPID PLA plus filament features high flexural modulus and elongation at break, which makes it resistant to brittleness and cracking, bringing excellent results for printing functional parts
LESS-TANGLE & NEATLY WOUND: Full mechanical winding and strict manual inspection ensures that all high-speed pla plus filaments are neatly wound, which effectively reduces tangles, snap and line breakage issues
TOP-NOTCH ACCURACY & CONSISTENT: Precise production process guarantee the filament of 1.75mm diameter, accuracy of +/- 0.02mm. Strict tolerances and perfect dimensional accuracy ensure smooth and consistent feeding for filaments
FOR MOST 3D PRINTERS: Rapid PLA+ filament fit for both regular printers and high speed printers, perfectly for most high speed printer such as Neptune 4, Neptune 4 pro, K1, K1 Max, Ender 5 series, Kobra 2, M5, M5C and more
Perfect Match for Every Need
Find your perfect match. Whether you value effortless printing, incredible strength, blazing speed, or tough durability, our range of PLA, PLA Plus, Rapid PLA Plus, PETG, and Rapid PETG has you covered.
| PLA | PLA Plus | Rapid PLA Plus | PETG | Rapid PETG | |
| Nozzle Temperature |
190 – 230 °C
|
200 – 230 °C
|
200 – 230 °C
|
230 – 260 °C
|
240 – 270 °C
|
| Bed Temperature (Varies by Printer & Plate Type) |
35 – 65 °C
|
35 – 65 °C
|
35 – 65 °C
|
65 – 75 °C
|
65 – 75 °C
|
| Printing Speed |
< 300 mm/s
|
< 280 mm/s
|
< 600 mm/s
|
< 250 mm/s
|
< 600 mm/s
|
| Tensile Strength–XY |
38 ± 3 MPa
|
38 ± 2 MPa
|
39 ± 2 MPa
|
37 ± 2 MPa
|
42 ± 2 MPa
|
| Impact Strength–XY |
66.2 ± 3.9 kJ/m²
|
65.5 ± 3.6 kJ/m²
|
50.4 ± 2.8 kJ/m²
|
55 ± 3.1 kJ/m²
|
87.6 ± 4.2 kJ/m²
|
| Bending Strength–XY |
72 ± 5 MPa
|
74 ± 4 MPa
|
71 ± 6 MPa
|
65 ± 2 MPa
|
68 ± 2 MPa
|
| Bending Modulus–XY |
2993 ± 182 MPa
|
2979 ± 156 MPa
|
2846 ± 175 MPa
|
1946 ± 105 MPa
|
2097 ± 173 MPa
|
| Breaking Elongation Rate–XY |
10.5% ± 2.1%
|
7.9% ± 1.6%
|
8.5% ± 1.2%
|
6.9 ± 1.6%
|
8.9% ± 1.5%
|
| Heat Deflection Temperature |
57 °C
|
56 °C
|
57 °C
|
69 °C
|
72 °C
|